Variation in wall thickness occurs due to _________ core boxes.

(a) Rigid

(b) Flexible

(c) Surface finished

(d) Worn out

This question was posed to me during an online exam.

Question is from Casting Defects topic in portion Concept of Gating and Risering of Foundry and Forging

1 Answer

+1 vote
by (736k points)
selected by
 
Best answer
The correct choice is (d) Worn out

The best explanation: Worn out core boxes give oversize core dimensions. Worn out core prints allowing a core to float or move. Inadequate core print areas permit lifting of the core due to the buoyancy of molten metal. Hence the variation in wall thickness occurs.

Related questions

We welcome you to Carrieradda QnA with open heart. Our small community of enthusiastic learners are very helpful and supportive. Here on this platform you can ask questions and receive answers from other members of the community. We also monitor posted questions and answers periodically to maintain the quality and integrity of the platform. Hope you will join our beautiful community
...