+1 vote
in Foundry and Forging by (110k points)
__________ usually occurs at the parting line and results in excess of metal.

(a) Fins

(b) Fash

(c) Strain

(d) All of the mentioned

I have been asked this question during an interview.

This interesting question is from Casting Defects topic in section Concept of Gating and Risering of Foundry and Forging

1 Answer

+1 vote
by (736k points)
selected by
 
Best answer
Right answer is (d) All of the mentioned

The best explanation: The fins, fash and strain all occur due to the same reason. They occur at the parting line. Straining or movement of the mould makes a casting appreciably thicker than the pattern. Hence, at the parting line excess metal is accumulated which is to be grounded off.

Related questions

We welcome you to Carrieradda QnA with open heart. Our small community of enthusiastic learners are very helpful and supportive. Here on this platform you can ask questions and receive answers from other members of the community. We also monitor posted questions and answers periodically to maintain the quality and integrity of the platform. Hope you will join our beautiful community
...