Which of the following characteristic is not expected in the green sand in the green sand molding process?

(a) Flowable nature

(b) Plastic Nature

(c) Reactivity

(d) Permeability

This question was posed to me during a job interview.

The doubt is from Green Sand Moulding in chapter Moulding Machines & Special Moulding Processes of Foundry and Forging

1 Answer

+1 vote
by (736k points)
selected by
 
Best answer
Right option is (c) Reactivity

Easy explanation: If the green sand develops the quality of reactivity in it, it will have significant defects in it which will result in discarding of the entire casting. Hence all the qualities except reactivity are desired in the sand.

Related questions

We welcome you to Carrieradda QnA with open heart. Our small community of enthusiastic learners are very helpful and supportive. Here on this platform you can ask questions and receive answers from other members of the community. We also monitor posted questions and answers periodically to maintain the quality and integrity of the platform. Hope you will join our beautiful community
...