+1 vote
in Foundry and Forging by (110k points)
Uncontrolled permeability in the green sand mould leads to ___________

(a) Blow Holes

(b) Chills

(c) Shrinkage

(d) Tearing

The question was posed to me in class test.

I need to ask this question from Types of Sand Moulds in chapter Pattern Materials & Moulding Sand Tests of Foundry and Forging

1 Answer

+1 vote
by (736k points)
selected by
 
Best answer
Right option is (a) Blow Holes

Explanation: The rate of flow of air passing through a standard specimen under a standard pressure is termed as a permeability number. The permeability of these holes should be properly controlled, otherwise blow holes and gas inclusions are likely to form.

Related questions

We welcome you to Carrieradda QnA with open heart. Our small community of enthusiastic learners are very helpful and supportive. Here on this platform you can ask questions and receive answers from other members of the community. We also monitor posted questions and answers periodically to maintain the quality and integrity of the platform. Hope you will join our beautiful community
...